Issued by Engineers & Architects after earthquake group
(http://on.fb.me/1zJqpHC)
Plaster Cracks
Below 10 mm.Material : Doctor Fixit Crack ‘X’ Paste
Procedure :
- 1. First cut the crack with ‘V’ Shape
- 2. Clean the crack area.
- 3. Moisture the crack area.
- 4. Apply the crack paste by running hand.
- 5. Leave it by
Below 5 mm.
Material : Crack ‘X’ Paste Shrink Free
Procedure :
- 1. First cut the crack with ‘V’ Shape
- 2. Clean the crack area.
- 3. Moisture the crack area.
- 4. Apply the crack paste by running hand.
- 5. Leave it by
Concrete Crack
Material: Doctor Fixit Crack Super latest
Procedure:
First mix the solution of Doctor Fixit : Water : Cement in the ratio of 1 : 4 : 7 (i.e. if you use 100 grams of Doctor Fixit use 400 milliliters (grams) of water and 700 grams of cement)
Or
Mix the solution of cement and sand in the ratio of 1:3 and add Doctor Fixit Solution 20 % of the cement volume (i.e. if you use 1 Kg of cement then use 200 grams of the Doctor Fix it Solution)
And then
1. First cut the crack with ‘V’ Shape
2. Clean the crack area.
3. Moisture the crack area.
4. Apply the crack paste by running hand.
5. Leave it by
Thank you for sharing your thoughts and knowledge on this topic. This is really helpful and informative, as this gave me more insight to create more ideas and solutions for my plan. I would love to see more updates from you.
ReplyDeleteElcometer